Day plot data of hysteresis parameters of representative samples for VER98-1-14, VER98-1-1 and VER98-1-3

The day plot (Fig. 6B; Day et al., 1977) indicates that samples with S-ratios >0.95 plot rather in the single-domain (SD) to pseudosingle-domain (PSD) range. Samples with S-ratios between 0.9 and 0.95 instead, plot rather in the PSD to the multidomain (MD) range. Low S-ratio samples are not greatly dispersed and have ratios of Bcr/Bc and Mrs/Ms of 3.5 and 0.1, respectively.

High temperature measurement of the saturation magnetisation for VER98-1-14

It shows a loss of a part of the signal at temperatures between 350 and 400 °C, typical disintegration temperatures for greigite. The remaining signal disappears above a temperature of 590 °C, typical for magnetite.

High temperature measurement of the saturation magnetisation for VER98-1-1

It shows a loss of a part of the signal at temperatures between 350 and 400 °C, typical disintegration temperatures for greigite. The remaining signal disappears above a temperature of 590 °C, typical for magnetite.